Abstract

In order to reduce shading loss and keep low Rs under fine-line printing process, front-side metallization with high aspect ratio is necessary. In this paper, stencil screen with several opening widths are compared with mesh screen. While opening width in mesh screen is confined to about <;40um, cells with high series resistance are generated because of the low cross section area of the finger. Nevertheless, stencil printing with 100% open areas could raise the aspect ratio in fine-line printing and effectively improve finger uniformity, leading to lower series resistance. In this work, fingers with aspect ratio over 0.5 have been achieved by stencil printing and kept low width. On the other hand, five pastes with different viscosity are applied to optimize stencil printing for 35μm and 45μm opening width respectively. The paste with higher viscosity has larger aspect ratio but poor printing quality. Finally, through line resistance measurement, larger aspect ratio performed by stencil printing actually exhibits lower resistance than that by mesh printing, making stencil suitable in fine-line printing production. With stencil printing for only fingers, followed by mesh printing of the busbars, +0.06% efficiency gain was achieved compared with single mesh printing as the result of the low resistance and high FF.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.