Abstract
Ultra-high molecular weight polyethylene nanocomposite coatings reinforced with 1 wt.% graphene nanoplatelets were deposited on aluminum substrates. Sliding wear tests with a pin-on-disc configuration were conducted at different temperatures (25oC, 75oC, 90oC, 115oC, and 125oC) to evaluate the wear behavior of the coating at elevated temperatures. The ultra-high molecular weight polyethylene/1 wt.% graphene nanoplatelets nanocomposite coating showed an outstanding performance by passing the wear test without failing even until temperatures of 115oC as compared to the pure ultra-high molecular weight polyethylene coating which failed at a much lower temperature of 75oC, indicating an improvement in the operating temperature range of ultra-high molecular weight polyethylene by at least 44%.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Proceedings of the Institution of Mechanical Engineers, Part J: Journal of Engineering Tribology
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.