Abstract

Abstract BZN-based ceramics with low sintering temperature were prepared using a conventional route. Green sheets of ceramics were formed using tape casting technique. The laminated tapes were pressed together for forming multilayer microwave resonators. The green chips were sintered at about 950 °C. In order to adjust the resonant frequency of resonator, the width of the ground terminal electrode of the stripline can be changed. When the width of the ground terminal electrode varied from 1.0 to 2.4 mm, the resonant frequency of resonator changed from 0.971 GHz to 0.986 GHz. As the width of the ground terminal electrode increased, the resonant frequency of resonator varied slowly and then saturated. The maximum adjusting value of the resonant frequency of resonator is about 1.5%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.