Abstract

This work presents results of investigation of crossed-field demagnetization in 2G high temperature superconducting stacks at temperatures in the range of 77 - 20 K and in a variable frequency, corresponding to the particular rotor application.We propose a method to reduce the demagnetization rate for a given stack configuration necessary for the superconducting rotor operating at a cryogenic temperature. This technique involves 3-D wrapping the stack of tapes with perpendicular layers of similar superconducting properties.Previous ‘proof of concept’ studies documented some improvements in flux demagnetisation reduction for basic configuration. In the present study a more advanced approach based on magnetic flux shielding is adopted. The presented results provide an important contribution to development for design solutions that aim to increase the operational time before remagnetisation of the stacks would be required.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.