Abstract

Two different clay loadings were added to OPEFB/PP/MAPP which was 7 phr and 10 phr in order to see its effect on the fracture toughness. Standard dimension of samples was prepared for 180 μm, 355 μm and 355 μm treated with 1% NaOH. The result showed that 7 phr clay contents had the highest fracture toughness of 1.16 MPa.m1/2. Alkali treatment on OPEFB fiber gave 7% improvement of fracture toughness for samples with 7 phr PPnanoclay loading. SEM images show the improvement of bonding between the fibers and the matrix upon alkali treatment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.