Abstract

To evaluate the load at fracture and influence of artificial aging of posterior teeth occlusal veneers ("table tops") made of two different ceramics. A total of 80 table tops were produced from feldspathic ceramic (VM) and zirconia-reinforced lithium silicate ceramic (CD) using computer-aided design/computer-assisted manufacturing (CAD/CAM). Half of the specimens from each ceramic were aged prior to the load test. Mean ± standard deviation (SD) load at fracture was significantly higher for CD (1,571.1 N ± 297.0 N) than for VM (573.6 N ± 86.4 N) (P < .001). After aging, load at fracture increased significantly to 1,819.0 N (± 310.6 N) for CD and to 745.2 N (± 168.3 N) for VM. The use of zirconia-reinforced lithium silicate ceramic for molar nonprep table tops should be uncomplicated according to the high load-at-fracture values. Mechanical stability of either ceramic is not compromised by aging.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.