Abstract

The influence of loading type on tensile and tearing fracture resistance of ballast rock was assessed using edge-notched diametrically compressed disc (ENDC) and edge-notched disc bend (ENDB) test geometries. The geometry of these two specimens was similar; however, their loading type (i.e., three-point bend and diametral compressive) was different affecting the geometry factors. The obtained pure tensile fracture toughness (KIc) using the ENDB test was higher than the ENDC test. In contrast to tensile fracture toughness, the pure tearing fracture toughness (KIIIc) in the ENDC test was higher than the ENDB fracture test. The obtained experimental data were explained in terms of crack propagation path, since two distinct trajectories were observed for both configurations under tearing deformation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.