Abstract
Although materials generally become more ductile with increase in temperature and decrease in strain rate, many metals have a local minimum in ductility at specific temperatures and strain rates. There is thus a region where a decrease in stress level results in a decrease of elongation before fracture. Failure is observed to occur at interfaces and particularly at grain boundaries nearly perpendicular to the maximum principal tensile stress. The nucleation of cavities and cracks, however, appears to arise initially from shear processes at these interfaces at temperatures and stresses where grain boundary sliding is significant but transverse boundary movement is negligible. Thus, tensile and shear stresses play different roles. Since cavities have a finite volume and link together to cause failure, the hydrostatic component of stress is important and so, in evaluating criteria for fracture, a precise definition of the stress system is necessary. Further, chemical composition, segregation and microstructural features play a vital role and materials that are only slightly different may show quite dissimilar behaviour.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Philosophical Transactions of the Royal Society of London. Series A, Mathematical and Physical Sciences
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.