Abstract
The results of wear of four ceramic materials made of a partially stabilized zirconia (Y-TZP, YPCZ, Ce-TZP and Mg-PSZ) during friction against steel without lubrication are presented. It is shown that wear of ceramics from Y-TZP, Y-PSZ, and Ce-TZP occurs in two stages: first it’s a tear fracture and then it’s a shear fracture. The ceramics based on Mg-PSZ wears out by only the mechanism of shear fracture. Proceeding from the analysis, it was concluded that the wear mechanism of the ceramics under study depends on the grain boundary strength.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.