Abstract
Using a variety of advanced ceramic materials, a comparison has been conducted of fracture toughness test methods using the single edge vee-notch beam method and the surface crack in flexure method, the latter restricted to optical fractography. Good agreement has been found between the two methods on materials which were amenable to the SCF method. It has further been shown that the SEVNB method can produce reliable results on materials to which the SCF method is not readily applicable.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.