Abstract
The mechanical properties of inviscid melt spun (IMS) CaO-Al2O3 (46.5 wt % CaO-53.5 wt % Al2O3) eutectic fibres were examined by fractographic analysis as well as four-point bending and micro-indentation. The averaged fracture strength and elastic modulus values of the IMS Calcia-Alumina (CA) fibre were determined to be 460 MPa and 99.8 GPa, respectively by using four-point bending tests. The inner mirror constant (M) was determined to be 2.39 MPa·m1/2 by using the plot of the fracture strength (σf) obtained from the bending tests as a function of r−1/2, where r is the inner mirror radius measured from scanning electron microscopy (SEM) on the fractured CA fibres. The flaw-to-mirror ratio (c/r) for the CA fibre was calculated to be 1∶11.24. Also, the critical flaw size (c) of the CA fibre was estimated to be 2.35 μm. The averaged elastic modulus value from Knoop micro-indentation was determined to be 102.5 GPa which is in good agreement with that from the four-point bending tests.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have