Fractal study was used to the analysis of the fractured surface of commercial N50-type Nd-Fe-B sintered magnets. The strain-stress properties of the specimens indicate that the elastic and plastic deformations occur simultaneously during intergranual cracking. The microfractography of the specimens exhibits typical brittle fracture pattern with some toughness dimples, indicating that plastic deformation has happened in some local areas. A “line-measuring dimension” Dline was selected to discuss the fracture behavior. The calculated Dline is about 1.28 and 1.29 for the specimens with c-axis parallel and perpendicular to the applied force direction, respectively. The line-measuring dimension analysis indicates that the fracture feature may be isotropic for our studied specimens, which is a bit inconsistent with previous report on the fracture characterization of Nd-Fe-B sintered magnets. More comprehensive fractal study is further needed to confirm the fracture behavior in detail in the future.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.