Poly[1-(trimethylsilyl)-1-propyne] (PTMSP) dense films were evaluated for n-butanol recovery from aqueous solutions and acetone–butanol–ethanol (ABE) fermentation broth. Flux decline through PTMSP dense films due to polymer compaction under vacuum conditions, relaxation in alcohol and alcohol/water mixtures, and membrane contamination are discussed. Flux decline of a PTMSP film during pervaporation of 20 g/l BuOH/water mixture was fitted to the following function, y= At − b . PTMSP films change their geometry when exposed to alcohol and alcohol/water mixtures and then dried. As a result of the relaxation process, polymer film becomes thicker and denser, effecting membrane performance. PTMSP films that were treated with 70% iso-propanol/water show linear flux decline versus pervaporation time. Strong lipid adsorption seems to occur on the membrane surface when fermentation broth is used as a feed causing flux decline within short period of time.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.