Abstract

Effect of biofouling on various polymers and composites such as, Polyurethane (PU), Silicone rubber (SR), Polyester (PET), Glass Fiber Reinforced Polymer (GFRP), Carbon fibre Reinforced Plastic (CFRP) and Syntactic foams (SF) deployed for a period of one year in marine waters at a depth of 1 m was studied. These materials find wide marine applications. SR with lowest surface energy was the least fouled. Maximum barnacle attachment was seen on hard surface (GFRP) and minimum on flexible surface (SR). Attachment of barnacles and polychaetes are positively correlated with surface energy. Fouling load is positively correlated with Surface energy and hardness. The surface energy, hardness and tensile strength reduced while surface roughness considerably increased during this period. Maximum gravimetric weight loss was seen in PET (7.49%) followed by PU (4.25%) and minimum in CFRP (0.45%). Maximum thermogravimetric weight loss was observed in PET (73.5% at 400 °C) followed by PU (71.1%) and least in SR (2.4%). Fourier Transform infrared spectrum revealed that carbonyl/oxidation indices decreased for PET, GFRP, CFRP, and SR indicating biotic degradation. The same index increased for PU indicating abiotic oxidation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.