Abstract

Previous Electron Paramagnetic Resonance (EPR) studies identified the carbon dangling bond center as the main paramagnetic interface defect in 3C, 4H, 6H-SiC/SiO2. We demonstrate that this defect, called PbC center, can be passivated by forming gas annealing at 400°C. We have measured the PbC density at annealed 4H- and 3C-SiC/SiO2 interfaces and attributed its reduction to the transformation of the dangling bonds into EPR inactive C-H bonds. We have also studied the reverse phenomenon occurring during vacuum annealing at temperatures ranging from 600°C up to 1000°C and have determined a dissociation energy of ≈4.3 eV for the 3C and 4H polytypes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.