In the temperature range of approximately 110–130 K the transition of the planar slip to the wavy one occurs in AgCl crystals. The transition manifests itself by substantial shortening of originally long and straight slip traces on the top oriented surface of the samples. The wavy slip bands (in the bulk of the sample) are created by mutual association of the narrow, straight and long slip strips.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.