In this work, Ti25Cu75 melt-spun partially amorphous alloy was used as a source of Ti and Cu to synthesize in-situ TiC-Cu nanocomposites. The reaction between the alloy and carbon started during ball milling and continued during Spark Plasma Sintering. At the same time, during ball milling, the alloy experienced phase transformations: crystallization of the amorphous phase was followed by decomposition of TiCu3. Copper crystallites formed during the alloy transformations were the reason for the presence of copper regions 0.5–1 µm in size free from TiC nanoparticles in the sintered composites. The Ti-Cu intermetallics transformed into non-agglomerated TiC 10–20 nm in size distributed in the copper matrix. The hardness of the synthesized TiC-Cu nanocomposites exceeded that of composites obtained by conventional sintering of ball-milled Ti-C-Cu powders.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.