Abstract

Spindle-shape goethite (a-FeOOH) extremely fine particles were produced by air oxidation of an aqueous suspension consisting of a mixture of FeS04 and Na2CO3 at 30-40°C, using a standard-type bubble column. The time dependences of the fractional oxidation of total Fc(II7rpar; were measured under various combinations of experimental conditions. The shape and size (i.e., major and minor axes) of prepared a-FeOOH particles were observed with the aid of transmission electron microscopy. From such measurements and observations, the mechanism of spindle-shape a-FeOOH particle formation was deduced; the total number of a-FeOOH nuclei is fixed in the early stage of the oxidation reaction, and subsequently, only the particle growth tends to take place until leading to the final size, depending on the reaction condition, i.e., reaction rate.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.