Abstract

The calcium phosphate composite octacalcium phosphate / calcite was obtained at pH 5–7 from the CaCO3/Ca(H2PO4)2 aqueous suspension in a galvanostatic mode at a current density of 20 mA/cm2 for 20 min. Drying at 80 °C without the precipitate maturation stage led to a powder formation consisting of brushite, calcite and a small amount of octacalcium phosphate. Prolonged maturation in air for 2 months led to the hydrolytic transformation of brushite into octacalcium phosphate stabilized by calcite. The use of electric current made it possible to increase the amount of octacalcium phosphate in the composite powder with the morphology of lamellar rosettes. Calcination at 800 °C of the composite powders led to the formation of α/β-tricalcium phosphate, β-calcium pyrophosphate, hydroxyapatite, and calcium oxide.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.