Abstract

A new technique of introducing mechanical vibration during isothermal holding period of hypoeutectic Al–Si alloy to prepare semi-solid slurry has been studied. The convection of melt caused by vibration had notable effects on the formation of near-spherical primary Al particles. When the vibrating frequency increased from 11.7 to 33.3 Hz, the average diameter of non-dendritic primary particles decreased from 125 to 90 μm, and the average shape coefficient increased from 0.40 to 0.55.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.