Abstract

In the present study, friction spot welding has been used for joining dissimilar AA5754 aluminum to AZ31 magnesium alloys. To get more insight into the microstructure, stop-action experimentation was employed. The welding cycle was forced to stop during the dwell time, and subsequently, the weld was quenched by pouring a mixed solution of ice and water to freeze the microstructure. Formation of the liquid phase leading to a formation of brittle intermetallic compound has been studied. Microstructural analyses reveal that formation of intercalated layers and a high density of grain boundaries induced by plastic deformation enhance the formation of eutectic structure during the welding process.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.