Abstract

The structure of layers and formation of intermetallic phases after thermal treatment in the system of thin electrodeposited Sn, Ni-Fe and sputtered Cu, Fe-Ni layers (thickness 0.1-2.0 μm) and thick electrodeposited Sn (thickness 6-10 μm) and Fe-Ni and Ni-B layers (thickness 2 μm) have been investigated by means of scanning electron microscopy (SEM), transmission electron microscopy (TEM), and by metallographic and X-ray diffraction (XRD) techniques. The formation of intermetallic phases NiSn3, Ni3Sn2, FeSn2 and considerable reduction in the formation of brittle layers Ni3Sn4, Cu6Sn5, Cu3Sn are determined by the structure and purity of electrodeposited tin [C (0.5-5) x 10-2; N (1-5) x 10-2; Fe, Cu, Bi, Pb (0.15-5.0) x 10-2 wt%] in the system Sn/Fe-Ni/Cu. Electrodeposited Fe-Ni (80% Ni) as barrier layer in the system Sn/Fe-Ni/sputtered Cu completely prevents formation of Cu6Sn5, Cu3Sn as a result of thermal treatment at 170°C up to 75 h. An amorphous Ni-B layer [B 4-8; C (3-7) x 10-2 wt%] prevents formation of Ni3Sn4 and Cu6Sn5 in the system Sn/Ni-B/Cu (or Cu-Zn alloy) as a result of thermal treatment at 130°C (200 h) and 170°C (150 h).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.