Abstract
Beta-Ti alloys contain sufficient concentrations of β stabilizing alloy additions to permit retention of the metastable β phase after cooling to room temperature. Decomposition of the metastable β phase results in the formation of several possible phases, at least two of which are metastable. Concurrently, equilibrium α phase often forms first by heterogeneous nucleation at the α grain boundaries with an accompanying precipitate free zone observed adjacent to the grain boundary α. The grain boundary regions are softer than the precipitation hardened matrix. As a consequence, fracture follows the prior β grain boundaries, especially in high-strength conditions. This fracture mode results in low tensile ductility and/or fracture toughness. This article will describe methods of minimizing or eliminating grain boundary α formation by using metastable transition precipitates to nucleate α more rapidly. The effects on fracture behavior also will be described.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.