Welding of titanium alloy TA15 to aluminum alloy Al 2024 was conducted by pulsed current gas tungsten arc welding using AlSi12 filler metal. Formation process of phases near the Ti/Al interface was discussed. Titanium and aluminum were partially fusion welded in the upper part while brazed together in the middle and bottom parts of the joint. In the upper part of the joint, intermetallics Ti3Al + Ti5Si3, TiAl + Ti5Si3, and TiAl3 were formed as three layers orderly from the titanium side to the weld metal. In the middle and bottom parts of the joint, intermetallics Ti5Si3 and TiAl3 were formed as two layers near the Ti/Al interface.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.