We investigate the formation mechanism of stray grain of nickel-based single-crystal superalloy under a high magnetic field. It was shown that the high magnetic field induced the formation of stray grains on the side that the dendrite diverges the wall. In addition, results showed a sloping solid/liquid interface and a further increased sloping magnitude under a high magnetic field. Further, the formation process of stray grain in the high magnetic field is analyzed in detail.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.