Abstract
Based on Miedema’s model, the enthalpy of formation, excess free-energy and partial molar excess free-energy of Sn-Pb binary alloy solders were calculated. The model of the activity coefficient for each component in the solders was established. The diagrams of enthalpy of formation, free energy versus composition and activity versus composition and temperature as well as activity coefficients as a function of composition and/or temperature were drawn. And then the relationship between the activity coefficients of elements Sn/Pb in the solders and temperature was obtained. The approaches to reduction in the volatilization of lead at high temperature were proposed from the point of views that the lead pollution to environment results from its chemical activity in the solder alloys.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.