Abstract

Cavitation erosion often causes the leakage of water in piping systems of industrial plants. Cavitation erosion tests were carried out for S15C carbon steel equivalent to pipe steel STPG370 in a stationary specimen test method using a vibratory apparatus specified by ASTM G32-03. Another test was performed using a cavitating liquid jet method according to ASTM G134-95 to simulate the flow condition. It was found that the maximum depth of erosion (MaxDE) increases with exposure time with a power of about 0.5 which is different from the ordinary power of 1.0. The distribution of the maximum depth of erosion pits was obtained by the extreme value analysis (Gumbel distribution) at every exposure time.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.