Abstract

In the system of ZrO2-Al2O3, cubic ZrO2 solid solutions containing up to 40 mol% Al2O3 crystallize at low temperatures from amorphous materials prepared by the simultaneous hydrolysis of zirconium and aluminium alkoxides. At higher temperatures, they transform into tetragonal solid solutions. Metastable ZrO2 solid solution powders containing 25 mol% Al2O3 have been sintered at 1000–1150 °C under 196 M Pausing the hot isostatic pressing technique. The solid solution ceramics consisting of homogeneous microstructure with an average grain size of ≈ 50 nm exhibited a very high fracture toughness of 23 MN m −1.5. They have been characterized by X-ray diffraction and electron probe surface analyses.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.