Abstract
AbstractAlumina‐former coatings have been known as the best surface engineering approach to combat high temperature corrosion in gas turbine industry. In this investigation, attempts have been made to obtain a titanium‐modified aluminide coating with improved protective properties. Modification has been achieved by introducing titanium in the coating composition by a two‐stage coating treatment; titanium coating and subsequent aluminising. The modified coatings were characterised and compared with simple aluminides by means of electron metallography, depth elemental profiling and x‐ray diffraction techniques. Experimental results indicated that pre‐titanising diffusion treatment is an effective route to modify chemical composition of simple aluminide coating. The final microstructure of the coating was β‐NiAl matrix with titanium‐bearing precipitates mainly distributed in near surface layers. The mechanism of the coating formation is discussed. Copyright © 2009 John Wiley & Sons, Ltd.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.