Results of high-energy magnetic X-ray diffraction on pure antiferromagnetic chromium are presented. The temperature dependence of the propagation vector of the spin-density wave (SDW) and the strain-wave (SW) could be reproduced. The temperature dependence of the magnetic integrated intensity could be measured in the transversally as well as in the longitudinally polarised SDW phase. The magnetic form-factor has been determined in the transversally polarised SDW phase with five magnetic satellites. For the first time a spin-orbit separation has been performed by comparing X-ray to neutron data. The small orbital contribution to the magnetisation density turns out to be negligible, in agreement to our relativistic band-structure calculations. In addition, measurements of strain-wave reflections have been undertaken, and the results complement previous studies.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.