Abstract

This paper presents an assessment of recycling of thermally treated fluvial sediments as a supplementary cementitious material (SCM). Different calcination treatments were conducted with temperatures ranging between 450°C and 950°C. For each calcined sediment, a detailed characterization was carried out. Subsequently, blended cements containing 25% calcined sediments (CS) were prepared and tested, including portlandite consumption, hydration kinetics, and compressive strength development (41 and 52 MPa at 7 and 90 days, respectively). The results showed that blended cement based on CS at 750°C provided the most favorable hydration kinetics and the highest compressive strength. An optimization design of experiment was followed to maximize the substitution rate of CS. The resulting multivariable function suggests a replacement rate up to 20% to produce a blended cement equivalent to CEM II 52.5 N, and up to 30% to produce a cement equivalent to CEM II 42.5 N. The reported technoenvironmental findings corroborate the use of CS as SCMs and motivate future research on their effect on concrete properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.