Abstract
ABSTRACT Herein, we report the preparation and characterisation of fluororubber coated superhydrophobic Poly (ethylene tetrapthalate) (PET) fabric and polyurethane (PU) sponge. The coating surface structure over PET fabric is more stable and hydrophobic (water contact angle (CA) ≥ 153°) with mass ratio 5:1 of fluororubber/carbon nanotubes (CNTs). Fluororubber/CNT coated PET fabric has good wear resistance and hydrophobicity with repeated friction. PU sponge coated with the ratio 8:4 of fluororubber/carbon black (CB) is the best ratio showing water CA ≥ 157°. Fluororubber/CB coated PU sponge has good oil-water separation and repeated oil absorption ability. Its absorption ability to various solvents and oils can reach 20–50 times its own weight. The EMI SE of fluororubber coating in 8.2–12.4 MHz range has improved with the increased CNTs content. The highestEMI SE valuee, i.e. 52.30 db achieved at 2.0 wt% CNT content. Developed fluororubber superhydrophobic coating material has good potential in the EMI shielding application.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.