Abstract

To elucidate the behavior of fluoride evaporation in an electroslag remelting process, the non-isothermal evaporation of the low-fluoride CaF2-CaO-Al2O3-MgO-TiO2-(Na2O-K2O) slag is studied using thermogravimetric analysis. The evaporation law of the melted slag is further verified using thermodynamic calculations. Fourier transformation infrared (FTIR) spectroscopy is used to evaluate the change in slag structure. It is discovered that the principal evaporating substances are CaF2, KF, and NaF, while the evaporation of MgF2, AlF3, and AlOF is less. KF evaporates absolutely in the early stage of the reaction, and CaF2 evaporates in a large proportion during the late reaction period. At 1500 °C, the order of vapor pressure is KF > CaF2. When K2O and Na2O are added to the residue sample at the same time, the evaporation ability of KF is stronger than that of CaF2 and NaF. As the K2O content increases from 0 to 8.3 wt%, evaporation increases from 0.76% to 1.21%. The evaporation rates of samples containing more K2O and those containing more Na2O are 1.48% and 1.32%, respectively. Under the same conditions, K2O has a greater effect on evaporation than Na2O. FTIR results show that the addition of K2O depolymerizes the network structure and that K2O can depolymerize the network structure better than Na2O.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.