Abstract
Flotation separation of magnesite from dolomite in the presence of SSZS (sodium silicate modified with zinc sulfate) as an inhibitor and NaOL (sodium oleate) as a collector has been studied via flotation tests, zeta potential measurements, contact angle measurements, and Fourier transformation infrared spectroscopy analysis (FT-IR). The flotation tests show that NaOL has strong collecting capacity in magnesite and dolomite flotation, so it is difficult to separate two minerals via flotation without inhibitors. SSZS is used as the depressant, which can selectively inhibit dolomite flotation and has little depression effect on magnesite. Zeta potential measurements, contact angle measurements, and FT-IR analysis indicate that SSZS can adsorb strongly onto dolomite’s surface and has a weak adsorption effect on magnesite. The adsorption of SSZS prevents NaOL from acting on the surface of dolomite. On the contrary, because there is little adsorption of SSZS onto magnesite, NaOL can still adsorb onto magnesite’s surface.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.