Abstract

A hydroxamate collector AM28 is used in conjunction with Potassium Amyl Xanthate (PAX) to allow the flotation of the low-grade copper oxide ores from DongChuan Mine. A series of batch laboratory scale flotation tests are conducted for oxide copper minerals to establish the flotation response and the suitability of the collectors. From the rougher flotation tests performed, the highest copper recovery obtained is 78.9% at a concentrate grade of 2.5% using AM28 dosage of 740g/t and PAX dosage of 20g/t. With one stage of cleaning, the obtained copper grade increases to 9.6% with the copper recovery at 64.9%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.