Abstract

We have grown underdoped (x = 0.11, 0.12) and optimally doped (x = 0.16) La2–xSrxCuO4 single crystals by the traveling-solvent floating-zone technique. In order to prepare good quality cuprate crystals, we have made much effort to optimize the preparation procedures. For example, we haveadopted the sol–gel route to prepare a highly fine and homogeneous La2–xSrxCuO4 precursor powder for fabricating a very dense ceramic feed rod used for the floating-zone growth, and we have also used quite a slow growth rate. The high quality of the grown crystals has been verified by double-crystal x-ray rocking curves, with the full-width-at-half-maximum being only 113–150 arcseconds, which are the best data reported so far for La2–xSrxCuO4 crystals. The superconducting critical temperatures of the grown crystals are 30, 31 and 38.5 K for x = 0.11, 0.12 and 0.16 samples, respectively, according to magnetic measurements.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.