Abstract
Flexible white organic light-emitting devices (WOLEDs) with an emitting layer consisting of a porous red poly(2-methoxy-5-(2'-ethyl-hexyloxy)-1,4-phenylenevinylene) (MEH-PPV) polymer layer and a blue 4,4'-bis(2,2'-diphenylvinyl)-1,1'-biphenyl (DPVBi) small molecular layer were fabricated on polyethylene terephthalate substrates. The current density of the flexible WOLEDs fabricated with a blend layer formed with a higher spincoating speed was significantly higher than that of a device fabricated with a lower spincoating speed, due to the higher pore density. The ratio between the red and the blue color peak intensities of the electroluminescence spectra for the flexible WOLEDs with a porous red MEH-PPV polymer layer and a blue DPVBi small molecular layer was controlled by the spincoating speed of the blend layer.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.