Abstract

Flexible film broadband absorber based on diamond-graphite mixture and polyethylene was fabricated by hot pressing. The film thickness of the absorber was 90 μm. We have measured angular reflectivity, diffusional reflectivity and transmittance in the range 85–8000 cm−1 (117–1.25 μm) in order to determine the absorption. It was shown that room temperature pressing of mesh print with 250 μm step significantly reduces reflectivity of the absorber. The absorption was over 0.85 in the range 85–320 cm−1 (117–31.25 μm) and >0.98 in the range 320–8000 cm−1 (31.25–1.25 μm). We believe that the designed and manufactured absorber might become a promising material for optical devices where high broadband absorption and flexibility are required.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.