Abstract
The paper presents the fire exposure, impact responses, and burst tests of glass-reinforced epoxy (GRE) composites pipes. Fire responses of three different fire exposure times (10 s, 20 s and 30 s) were conducted, followed by impact loadings. Three different energy levels (5 J, 7.5 J, and 10 J) were applied for impact responses and followed by monotonic burst tests. Monotonic burst tests were conducted on GRE samples using hydrostatic pressure testing equipment in accordance with ASTM D1599. The result shows that the longer the time of fire exposure towards GRE pipes, the higher the impact energy applied to the pipes, the lower the burst strength of the pipes. The maximum burst strength found decreased with an increase in the fire exposure time. The results also indicated that the strength of the GRE pipes significantly decreases with an increase in impact energy level.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.