Abstract

Abstract A finite-element model is proposed which describes the creep behaviour of a two-phase single-crystal superalloy. For the matrix phase, a user-defined material model is used. It describes the creep behaviour based on evolution equations for dislocation densities on individual slip systems. An interaction matrix determines the influence of one glide system on the other. Due to the face-centred cubic (fcc) symmetry, 9 independent parameters of the interaction matrix can be distinguished, describing slip on octahedral and cube glide planes with a Burgers vector of the type a/2 . The finite-element method (FEM) was used to describe the stress– strain behaviour as well as the dislocation evolution in matrix channels during creep deformation. Uniaxial stress in , , and directions was considered. The evolution of the calculated dislocation densities and the resulting creep curve are compared with experimental observations.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.