Abstract

In this paper, a finite element-based approach to the tube hydroforming process of SS304/CFRP material with different stacking sequences was performed in an effort to reveal the failure phases at different stacking angles. The effort to produce hybrid composite tubes through tube hydroforming with composite reinforcement resulted in laminate failure at all the proposed fiber orientation angles. A comparative study of strain energy dissipation at these different stacking angles is further presented. The results show that the 00/900 stacking is considered the strongest stacking angle requiring the least strain energy absorption to initial failure of approximately 50 % more as compared to the ±300 and ±600 stacking angles. The proposed method was more adequate for predicting the strain energy, matrix deformation, and fiber damage when simulating the events.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.