Abstract

ABSTRACT Cotton fabric was modified using polyacrylic rubber as a finishing agent in the presence of ammonium chloride, magnesium chloride, and sodium salts of phosphoric acid as catalysts, employing a pad-dry-cure technique. Treatment with 8% polyacrylic rubber in presence of 1.2% NaH2PO4, followed by drying of the padded fabric at 95°C for 5 min. and curing of the dried fabric at 140°C for 5 min., produced balanced improvements in properties such as tear strength, flexibility, tensile strength elongation at break, moisture regain, abrasion resistance, and wrinkle recovery. Functional group analysis and IR spectroscopy indicated that the NaH2PO4 catalyst allowed esterification of carboxyl groups of polyacrylic rubber with the cellulose constituents of cotton and the process ultimately led to some degree of crosslinking of the chain polymers of cotton.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.