Abstract
We developed an Al sputtering process by varying the plasma power, process temperature, and film thickness. We observed an increase of hillock distribution and average diameter with increasing plasma power, process temperature, and film thickness. Since the roughness of a film increases with the increase of the distribution and average size of hillocks, the control of hillock formation is a key factor in the reduction of Al corrosion. We observed the lowest hillock formation at 30 W and 100 oC. This growth characteristic of sputtered Al thin films will be useful for the reduction of Al corrosion in the future of the electronic packaging field.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.