Abstract

Ni nanopowders were sintered by a field-assisted sintering technique (FAST). The influence of heating rate from 90 to 1100 °C/min on densification and final grain structure of sintered Ni was studied. A moderate heating rate was found to be beneficial for the densification of Ni nanopowders, whereas a high heating rate was conducive to a lower final density. Very high heating rates resulted in non-uniform densification of the samples and formation of cracks during sintering. Electric field activation and possible densification mechanisms are discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.