Abstract

Nextel™ 720 fibers were coated with LaPO4 and CePO4 monazite. The coatings were applied using washed and unwashed rhabdophane sols derived from La(NO3)3/(NH4)2HPO4 and a washed sol derived from Ce(NO3)3/H3PO4. The coatings were cured in-line at 900°–1300°C. Multiple coatings were also applied. Fiber strength was retained after coating with washed sols, but not with unwashed sols. These results are consistent with earlier work on LaPO4 monazite fiber coatings derived from La(NO3)3/H3PO4.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.