Abstract

The study of laser bead-on-plate welding of nickel based superalloy Rene 77 using single mode high power fiber laser has been undertaken to determine the effect of process parameters, such as laser power, welding speed and laser beam defocusing, on the weld geometry and quality. Non-porous and crack-free welds can be achieved for a relatively wide range of fiber laser welding parameters. The welding speed has a major effect on the weld aspect ratio. The laser beam defocusing significantly affects the weld bead geometry, the stability of the keyhole and pore formation. The transition from keyhole mode to conduction mode welding occurs between focal point position +2.0 mm and +4.0 mm. The high porosity was observed at the focal point position of +2.0 mm. The heat input higher than18 J/mm results to hot cracking in the heat affected zone (HAZ). Moreover, it was found that the welds with the weld aspect ratio higher than 1.5 contain cracks, which propagate from the HAZ into the weld metal.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.