Ceramics based on barium aluminate with additives of iron (III) oxide and lithium hydroxide were obtained by solid-phase synthesis. It has been established that high-temperature treatment in an oxidizing medium contributes to the production of vacuum-dense samples that meet the «absolutely impermeable» tightness criterion, with a density of 3,75 g/cm3 , with a compressive strength limit of 597,1 MPa and a specific electrical conductivity in the range of 1,50·10‒7‒1,05·10‒4 Cm/ cm (at 90‒300 °C).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.