Abstract

The results studies influence physicochemical properties and thickness cover slag, formed during ladle desulfurization pig iron by blowing a mixture of lime and magnesium, features formation a breaker on the surface bath and the level of metal losses with emissions outside ladle from this zone are presented. The necessity creating conditions for ensuring height breaker, which would not exceed thickness slag layer on the surface bath, has been substantiated. Using results of the high-temperature simulation blowing the cast iron melt with a neutral gas supplied through the nozzles tips stationary and rotating submersible lances, features development of counter waves and metal splashes in the absence and during formation slag cover with thickness of 30—80 mm on the surface bath are determined. The features change in the height and area breakers are determined depending on the gas flow rate for blowing bath and thickness slag. Based on the analysis results low-temperature modeling bath blowing, scientific ideas about the combined effect of the bath blowing intensity, speed of rotation submerged lance and thickness slag layer on the diameter bubbling zone, gas saturation of the bath and features wave formation on its surface in the slag-free zone were further developed (so-called «eye»). The nature relationship between length of the gas jet from lance nozzle, diameter «eye», and geometric parameters breaker has been established. It is shown that dependence profile breaker on speed of rotation lance and thickness slag layer is nonlinear. So, blowing bath through tip of a rotating lance with one nozzle at 240 rpm. with a gas flow rate of 2.2 l/min. creates conditions for raising top breaker to a height that is 33 % higher than the current thickness slag layer and contributes to the intensification formation of waves and bursts on the surface bath. With a decrease in the gas flow rate to 1.0 l/min., Under other unchanged conditions, height breaker is already 2/3 of the height slag layer, and as thickness slag decreases proportionally decreases. The smallest, recorded in the experiments, relative height breaker was 33.3% of the slag thickness at a lance rotation speed in the range of 90—120 rpm. Mathematical models are proposed that are suitable for calculating height breakers depending on the thickness slag layer, speed of rotation lance and intensity of gas injection into the bath. Taking into account established mutually opposite effect thickness of the cover slag layer and speed of rotation submerged lance on the «eye» area and height of the breaker, it is advisable to continue search for ways to improve design tip submerged lance and slag mode of ladle desulfurization.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call