Abstract Large glassy alloy discs (12 mm diameter, 1 mm thickness) of high relative density (∼98%) were prepared by spark plasma sintering. The bulk magnetic cores (12 mm outer diameter, 6 mm inner diameter, 1 mm thickness) exhibit good soft magnetic properties: saturation magnetization is 1.44 T, coercivity is 31 A/m, and effective permeability at 1 kHz is 1320. They also exhibit much lower loss than a silicon steel core; core loss at 10 kHz and maximum induction of 0.2 T is only 81.7 W/kg.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.