Fe3O4-loaded ion exchange resin composites (Fe3O4@Resin) were optimally constructed through ion exchange and co-precipitation of Fe2+ and Fe3+ on strong acid ion exchange resin. The as-synthesized Fe3O4@Resin composite was characterized and investigated for 10B/11B separation including effect of pH and isotherms through batch adsorption experiments which can be well described by Langmuir model. In the chromatographic column packed with Fe3O4@Resin, 10B was selectively retained with a high dynamic separation factor of 1.312. Considering the consistency between simulated and experimental breakthrough curves within Fe3O4@Resin packed column, chromatographic 10B/11B separation performance was simulated under various conditions which were further optimized by Response surface methodology. Consequently, the annual yield of 10B reached the maximum of 2534 g with feed concentration of 9.729 g L−1, flow rate of 146.05 mL min−1, and column size of 2.2 × 150 cm (I.D. × length). In addition, five-cycle adsorption/regeneration experiments demonstrated its merit of reusability.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.